Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H07G-00 Polypropylene Homopolymer

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H07G-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade H07G-00 is a barefoot polypropylene homopolymer designed for cast film applications and flexible packaging. This grade has good optical properties and consistent processing. This grade meets the requirements of the U.S. Food and Drug Administration specified in 21 CFR 177.1520.
Physical Properties Metric English Comments
Density 0.909 g/cc
0.0328 lb/in³
ASTM D792
Melt Flow 7.53 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.53 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D785
Tensile Strength at Break 18.79 MPa
2725 psi
2 in/min; ASTM D638
Tensile Strength, Yield 36.0 MPa
5220 psi
2 in/min; ASTM D638
Elongation at Break 160 %
160 %
2 in/min; ASTM D638
Elongation at Yield 11 %
11 %
2 in/min; ASTM D638
Flexural Modulus 1.529 GPa
221.7 ksi
1% Secant; ASTM D790A
Izod Impact, Notched 0.283 J/cm
0.530 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.8 °C
199 °F
ASTM D648
Optical Properties Metric English Comments
Haze 25 %

@Thickness 1.30 mm
25 %

@Thickness 0.0512 in
75% Diffuse Transmission; ASTM D1003
Gloss 93 %
93 %
60° Angle; ASTM D2457
Descriptive Properties Value Comments
Process Film
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following: