Ineos H07B-01 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H07B-01 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a polypropylene homopolymer for cast film applications that require antiblock additives and nucleation. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsCast film for hot-pack cheese applicationsFlexible packagingBenefitsAntiblock additivesProcessabilityInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 7.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.3 MPa

@Temperature 23.0 °C
5850 psi

@Temperature 73.4 °F
ASTM D638
Flexural Modulus 2.02 GPa

@Temperature 23.0 °C
293 ksi

@Temperature 73.4 °F
ASTM D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648