Ineos H05M-00 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H05M-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade H05M-00 is a general purpose polypropylene homopolymer for injection molding applications. This resin provides good long-term heat stability. This material meets the requirements of the Food and Drug Administration as specified in CFR 21 177.1520.Suggested fabrication methods: Injection moldingFeatures: Long-term heat agingTypical applications: Appliances, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.
Physical Properties Metric English Comments
Density 0.886 - 0.926 g/cc
0.0320 - 0.0335 lb/in³
ASTM D1505
Water Absorption <= 0.010 %
<= 0.010 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cm
0.010 - 0.025 in/in
ASTM D955
Melt Flow 5.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79 - 108
79 - 108
Normal range for injection molding resins; ASTM D785
Tensile Strength, Yield 36.0 MPa
5220 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Elongation at Yield 9.0 %
9.0 %
ASTM D638
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790A
Izod Impact, Notched 0.200 - 0.300 J/cm

@Diameter 3.17 mm
0.375 - 0.562 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
UL Relative Thermal Index
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
ASTM D648
Flammability, UL94 HB
HB
Descriptive Properties Value Comments
Process Injection Molding