Ineos H03W-00 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H03W-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade H03W-00 is a homopolymer designed for extrusion processing. It exhibits low water carry over. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520Applications:Carpet backingWoven bagsTwineBenefits:Low water carry over
Physical Properties Metric English Comments
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa
4600 psi
D638
Elongation at Yield 9.0 %
9.0 %
D638
Flexural Modulus 1.31 GPa
190 ksi
D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
219 °F
D648
Descriptive Properties Value Comments
Process Extrusion
Fiber
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved