Material Notes:
This is a polypropylene homopolymer for biaxially oriented polypropylene (BOPP) film and blow molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsBOPPBlow moldingBenefitsExcellent film propertiesEase of processingInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.5 MPa

@Temperature 23.0 °C
4860 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Yield 12.9 %
12.9 %
ASTM D638
Flexural Modulus, 1% Secant 1240 MPa

@Temperature 23.0 °C
180000 psi

@Temperature 73.4 °F
0.05 in/min test speed
Izod Impact, Notched 0.534 J/cm

@Temperature 23.0 °C
1.00 ft-lb/in

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.1 °C
187 °F
ASTM D648