Ineos H03G-02 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H03G-02 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a homopolymer designed for fiber and tape applications requiring low water carryover and low die build-up. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsSlit TapeFilmFiberBenefitsLow water carryoverLow die build-upInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.7 MPa

@Temperature 23.0 °C
5470 psi

@Temperature 73.4 °F
ASTM D638
Flexural Modulus 1.59 GPa

@Temperature 23.0 °C
230 ksi

@Temperature 73.4 °F
ASTM D790A
Izod Impact, Notched 0.374 J/cm

@Temperature 23.0 °C
0.700 ft-lb/in

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101 °C
214 °F
ASTM D648