Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H02G-00 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Extrusion Grade , Polypropylene, Sheet/Thermoforming Grade
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H02G-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a low melt flow rate general purpose homopolymer polypropylene. This grade is designed to meet the processing and physical property requirements of sheet, film, and profile extrusion applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsConsumer ProductsIndustrial ProductsBOPP FilmExtrusion/ThermoformingBenefitsEase of processingHigh throughputGood balance of propertiesInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 2.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.51 MPa

@Temperature 23.0 °C
4715 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Yield 13.4 %
13.4 %
ASTM D638
Flexural Modulus, 1% Secant 1280 MPa

@Temperature 23.0 °C
185000 psi

@Temperature 73.4 °F
0.05 in/min test speed
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Copyright © lookpolymers.com All Rights Reserved