Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos G60-25-144 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos G60-25-144 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ineos G60-25-144 is a high density polyethylene homopolymer typically used in the production of sheet extrusion and blow molded containers. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.962 g/cc
0.0348 lb/in³
ASTM D4883
Melt Flow 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Yield 31.0 MPa
4500 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 800 %
>= 800 %
2 in/min (50 mm/min); ASTM D-638
Modulus of Elasticity 1.344 GPa
194.9 ksi
ASTM D638
Flexural Modulus 0.861 GPa
125 ksi
ASTM D747
1.55 GPa
225 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 2.10 J/cm
3.93 ft-lb/in
ASTM D256
Tensile Impact Strength 258 kJ/m²
123 ft-lb/in²
Type L, ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 131 °C
268 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments