Material Notes:
Fortiflex® B35-150-134 is an intermediate density polyethylene copolymer developed for injection blow molding. It exhibits excellent gloss and environmental stress crack resistance (ESCR) in molded containers. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.This product information was provided by Solvay Polymers, now a part of the BP Solvay Polyethylene North America joint venture (Nov. 2001).This product is not listed in the standard Innovene product line. The polypropylene and polyethylene products of BP Amoco have been moved to the Innovene Division in 2005. BP Amoco acquired the Fortiflex® Polyethylene product line from Solvay Polymers in November 2001.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D4883
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength, Yield 18.6 MPa
2700 psi
ASTM D638
Elongation at Break 950 %
950 %
ASTM D638
Flexural Modulus 0.750 GPa
109 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 5.60 J/cm
10.5 ft-lb/in
ASTM D256
Tensile Impact Strength 353 kJ/m²
168 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 58.0 °C
136 °F
ASTM D648
Vicat Softening Point 120 °C
248 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746