Ineos ABS Triax® DP 3155 ABS + Polyamide Blend (Conditioned)  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Nylon
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Triax® DP 3155 ABS + Polyamide Blend (Conditioned)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Features:Contains FillerSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
(DAM)
Water Absorption 4.3 %
4.3 %
(from DAM)
Moisture Absorption at Equilibrium 0.95 %
0.95 %
23°C/50% R.H. (from DAM)
Linear Mold Shrinkage, Flow 0.0080 cm/cm
0.0080 in/in
Linear Mold Shrinkage, Transverse 0.010 cm/cm
0.010 in/in
Melt Flow 8.0 g/10 min

@Load 5.00 kg,
Temperature 280 °C
8.0 g/10 min

@Load 11.0 lb,
Temperature 536 °F
cm³/10 min.
Mechanical Properties Metric English Comments
Tensile Modulus 2.00 GPa
290 ksi
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
DAM
CTE, linear, Transverse to Flow 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
DAM
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
(from DAM)
Vicat Softening Point 163 °C
325 °F
50°C/h 50N (from DAM)
Processing Properties Metric English Comments
Melt Temperature 260 °C
500 °F
Injection Molding
Mold Temperature 80.0 °C
176 °F
Injection Molding
Injection Velocity 40.0 mm/sec
1.57 in/sec