Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, As Conditioned  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend , Nylon
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS TRIAX® 1408 GF ABS/Nylon Blend, Injection Grade, As Conditioned  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Standard injection molding grade, easy flow, easy mold release, fast setting.Applications: Thin walled engineering parts. Automotive sector: air filters, switch and connector parts for car electric. Electrical sector: switch and connector partsInformation provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Dry As Molded
Mechanical Properties Metric English Comments
Elongation at Break 10 %
10 %
Charpy Impact Unnotched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 1.60 J/cm²
7.61 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 117 °C
243 °F
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F