Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos ABS Lustran® SAN DN79 SAN Grade

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded
Manufacturer Ineos ABS
Trade Name Lustran®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Lustran® SAN DN79 SAN Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lustran® SAN DN79 is a natural color, styrene-acrylonitrile copolymer supplied in pellet form. It is designed for used in compounding.
Physical Properties Metric English Comments
Melt Flow 7.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
7.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 79.3 MPa
11500 psi
ASTM-D638
Flexural Strength 96.5 MPa
14000 psi
at Fail; ASTM-D790
Flexural Modulus 3.62 GPa
525 ksi
ASTM-D790
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Vicat Softening Point 111 °C

@Load 1.00 kg
232 °F

@Load 2.20 lb
120°C/hour; ASTM-D1525
Descriptive Properties Value Comments
Acrylonitrile Content (%) 32.5
Users viewing this material also viewed the following: