Material Notes:
Lustran® ABS 786 resin is a black, virgin extrusion grade of ABS (acrylonitrile butadiene styrene). It is designed for extruded drain, waste, and vent (DWV) pipe. Lustran® ABS 786 (901046 black) resin meets or exceeds ASTM D 3965 4-2-2-2-2 cell class requirements for ASTM F 628 and D 2661. It is also listed under NSF Standard 14.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM-D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.0 MPa
4930 psi
ASTM-D638
Tensile Modulus 1.90 GPa
276 ksi
ASTM-D638
Izod Impact, Notched 4.00 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
7.49 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM-D256
5.87 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
11.0 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C

@Thickness 6.35 mm
212 °F

@Thickness 0.250 in
Annealed; ASTM-D648
Processing Properties Metric English Comments
Melt Temperature 221 - 232 °C
430 - 450 °F
Extrusion
Drying Temperature 82.0 - 93.0 °C

@Time 7200 sec
180 - 199 °F

@Time 2.00 hour
Moisture Content <= 0.050 %
<= 0.050 %
Dew Point <= -29.0 °C
<= -20.2 °F
inlet air
Descriptive Properties Value Comments
Screw Compression Ratio 2.4-2.8:1
Extrusion
Screw Length-to-Diameter Ratio 24-36:1