Material Notes:
Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
Melt Flow 10 g/10 min

@Load 10.0 kg,
Temperature 220 °C
10 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.3 MPa
5990 psi
Elongation at Break 25 %
25 %
Nominal
Elongation at Yield 3.3 %
3.3 %
Tensile Modulus 2.48 GPa
360 ksi
Charpy Impact, Notched 4.00 J/cm²
19.0 ft-lb/in²
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 88.0 µm/m-°C

@Temperature 20.0 °C
48.9 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
194 °F
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
Vicat Softening Point 97.0 °C
207 °F
50°C/h 50N
Processing Properties Metric English Comments
Melt Temperature 250 °C
482 °F
Injection Molding
Mold Temperature 60.0 °C
140 °F
Injection Molding
Injection Velocity 200 mm/sec
7.87 in/sec
Injection Pressure 55.0 MPa
7980 psi