Ineos ABS Lustran® 266 Specialty, Transparent  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos ABS Lustran® 266 Specialty, Transparent  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A clear injection molding grade of ABS. This transparent, general-purpose grade provides clarity and toughness with ease of processing. Used in housings, toys, lawn and garden applications, and various consumer products.Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with Lanxess in 2007. Subsequently Ineos acquired 100% of Ineos ABS. This product is no longer listed as a standard NAFTA product.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108
108
ASTM D785
Tensile Strength, Ultimate 29.0 MPa
4210 psi
ASTM D638
Tensile Strength, Yield 37.0 MPa
5370 psi
ASTM D638
Elongation at Break 48 %
48 %
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Flexural Yield Strength 58.6 MPa
8500 psi
ASTM D790
Flexural Modulus 1.80 GPa
261 ksi
ASTM D790
Izod Impact, Notched 1.80 J/cm

@Thickness 3.17 mm
3.37 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 121 µm/m-°C

@Temperature 20.0 °C
67.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C

@Thickness 12.7 mm
201 °F

@Thickness 0.500 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C

@Thickness 12.7 mm
180 °F

@Thickness 0.500 in
Unannealed; ASTM D648
UL RTI, Electrical 60.0 °C

@Thickness 1.60 mm
140 °F

@Thickness 0.0630 in
UL746B
UL RTI, Mechanical with Impact 60.0 °C

@Thickness 1.60 mm
140 °F

@Thickness 0.0630 in
UL746B
UL RTI, Mechanical without Impact 60.0 °C

@Thickness 1.60 mm
140 °F

@Thickness 0.0630 in
UL746B
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Optical Properties Metric English Comments
Refractive Index 1.52
1.52
ASTM D542
Haze 3.0 %
3.0 %
0.100 in; ASTM D1003
Transmission, Visible 86 %

@Thickness 2.50 mm
86 %

@Thickness 0.0984 in
ASTM D1003
Processing Properties Metric English Comments
Melt Temperature 205 - 230 °C
401 - 446 °F
Users viewing this material also viewed the following: