Material Notes:
Description: MC507U is a utility grade, glass fabric/silicone resin binder composite product that can be substituted for NEMA G-7, in most heating, appliance insulation and some bearing applications.MC507U has excellent strength and electrical properties.MC507U complies with MIL-I-24768/17 – GSG, with the exception of specific electrical properties.Thickness Tested: 0.500”
Physical Properties Metric English Comments
Density 1.88 g/cc
0.0680 lb/in³
Moisture Absorption at Equilibrium 0.040 %

@Thickness 3.17 mm
0.040 %

@Thickness 0.125 in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95 - 115

@Thickness 3.17 mm
95 - 115

@Thickness 0.125 in
Tensile Strength, Yield 138 MPa

@Thickness 3.17 mm
20000 psi

@Thickness 0.125 in
LW
Flexural Strength 207 MPa

@Thickness 3.17 mm
30000 psi

@Thickness 0.125 in
LW
Compressive Strength 345 MPa

@Thickness 3.17 mm
50000 psi

@Thickness 0.125 in
Flatwise
Izod Impact, Unnotched 10.1 J/cm

@Thickness 3.17 mm
19.0 ft-lb/in

@Thickness 0.125 in
LW, Cond E-48/50
Thermal Properties Metric English Comments
Decomposition Temperature >= 275 °C
>= 527 °F
Degradation Temperature
UL RTI, Electrical 170 °C
338 °F
UL RTI, Mechanical without Impact 220 °C
428 °F
Electrical Properties Metric English Comments
Volume Resistivity 4.00e+8 ohm-cm

@Thickness 3.17 mm
4.00e+8 ohm-cm

@Thickness 0.125 in
Surface Resistance 5.00e+8 ohm

@Thickness 3.17 mm
5.00e+8 ohm

@Thickness 0.125 in
Dielectric Constant 4.5

@Thickness 3.17 mm
4.5

@Thickness 0.125 in
Permittivity
Dielectric Strength 13.8 kV/mm
350 kV/in
Perpendicular - Short Time
Dielectric Breakdown 45000 V

@Thickness 3.17 mm
45000 V

@Thickness 0.125 in
Dissipation Factor 0.0035

@Thickness 3.17 mm
0.0035

@Thickness 0.125 in
Arc Resistance 240 sec

@Thickness 3.17 mm
240 sec

@Thickness 0.125 in
ASTM D495
Descriptive Properties Value Comments
Bond Strength 900 lb
0.5"