Indium Corp. Indalloy 84 Bismuth-Lead-Tin-Cadmium Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 84 Bismuth-Lead-Tin-Cadmium Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.63 g/cc
0.312 lb/in³
Thermal Properties Metric English Comments
Melting Point 132 - 139 °C
270 - 282 °F
Solidus 132 °C
270 °F
Liquidus 139 °C
282 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 5.0 %
5.0 %
Cadmium, Cd 18 %
18 %
Lead, Pb 32 %
32 %
Tin, Sn 45 %
45 %