Indium Corp. Indalloy® 8 In-Sn-Cd Fusible Alloy

Category Metal , Nonferrous Metal , Indium Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 8 In-Sn-Cd Fusible Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.46 g/cc
0.270 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 4.8

@Load 100 kg,
Time 30.0 sec
4.8

@Load 220 lb,
Time 0.00833 hour
Tensile Strength, Ultimate 18.1 MPa
2630 psi
Thermal Properties Metric English Comments
CTE, linear 24.0 µm/m-°C

@Temperature 20.0 °C
13.3 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 36.0 W/m-K

@Temperature 85.0 °C
250 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 93.0 °C
199 °F
Eutectic
Solidus 93.0 °C
199 °F
Liquidus 93.0 °C
199 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 14 %
14 %
Indium, In 44 %
44 %
Tin, Sn 42 %
42 %