Indium Corp. Indalloy 75 Bismuth-Tin Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 75 Bismuth-Tin Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.58 g/cc
0.310 lb/in³
Thermal Properties Metric English Comments
Melting Point 135 °C
275 °F
Eutectic
Solidus 135 °C
275 °F
Liquidus 135 °C
275 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 57.4 %
57.4 %
Lead, Pb 1.0 %
1.0 %
Tin, Sn 41.6 %
41.6 %