Indium Corp. Indalloy 69 Bismuth-Tin Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 69 Bismuth-Tin Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.58 g/cc
0.310 lb/in³
Thermal Properties Metric English Comments
Melting Point 95.0 - 129 °C
203 - 264 °F
Solidus 95.0 °C
203 °F
Liquidus 129 °C
264 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 51.6 %
51.6 %
Indium, In 6.0 %
6.0 %
Lead, Pb 5.0 %
5.0 %
Tin, Sn 37.4 %
37.4 %