Indium Corp. Indalloy 243 Tin Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 243 Tin Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lead-free alloy, no PatentInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 7.31 g/cc
0.264 lb/in³
Thermal Properties Metric English Comments
Melting Point 227 °C
441 °F
Eutectic
Solidus 227 °C
441 °F
Liquidus 227 °C
441 °F
Component Elements Properties Metric English Comments
Copper, Cu 1.0 %
1.0 %
Tin, Sn 99 %
99 %