Indium Corp. Indalloy 194 Gold Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 194 Gold Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 16.92 g/cc
0.6113 lb/in³
Thermal Properties Metric English Comments
Melting Point 370 - 800 °C
698 - 1470 °F
Solidus 370 °C
698 °F
Liquidus 800 °C
1470 °F
Component Elements Properties Metric English Comments
Gold, Au 98 %
98 %
Silicon, Si 2.0 %
2.0 %