Indium Corp. Indalloy 163 Tin-Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 163 Tin-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 11.2 g/cc
0.405 lb/in³
Thermal Properties Metric English Comments
Melting Point 299 - 304 °C
570 - 579 °F
Solidus 299 °C
570 °F
Liquidus 304 °C
579 °F
Component Elements Properties Metric English Comments
Lead, Pb 95.5 %
95.5 %
Silver, Ag 2.5 %
2.5 %
Tin, Sn 2.0 %
2.0 %