Indium Corp. Indalloy 148 Pure Bismuth

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 148 Pure Bismuth.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.80 g/cc
0.354 lb/in³
Thermal Properties Metric English Comments
Melting Point 271 °C
520 °F
Solidus 271 °C
520 °F
Liquidus 271 °C
520 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 100 %
100 %