Indium Corp. Indalloy 128 Pure Tin

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy , Pure Element
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 128 Pure Tin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 7.28 g/cc
0.263 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 13.1 MPa
1900 psi
Modulus of Elasticity 42.1 GPa
6100 ksi
Thermal Properties Metric English Comments
CTE, linear 24.0 µm/m-°C

@Temperature 20.0 °C
13.3 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.222 J/g-°C
0.0531 BTU/lb-°F
Solid
Thermal Conductivity 73.0 W/m-K

@Temperature 85.0 °C
507 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 232 °C
450 °F
Solidus 232 °C
450 °F
Liquidus 232 °C
450 °F
Component Elements Properties Metric English Comments
Tin, Sn 100 %
100 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000110 ohm-cm
0.0000110 ohm-cm