Indium Corp. 99.99% InI3 Indium Triiodide

Category Ceramic , Halide
Manufacturer Indium Corporation of America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 99.99% InI3 Indium Triiodide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Boiling Point: SublimesCrystalline Form: Carmine red or yellow crystalsIsomorphous with: AlCl3, YCl3Coordination Number: 6 Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 4.69 g/cc
4.69 g/cc
Solubility in Water 92.91 %
92.91 %
Molecular Weight 495.53 g/mol
495.53 g/mol
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.00010 - 0.0010 %
0.00010 - 0.0010 %
Cadmium, Cd 0.00050 - 0.0010 %
0.00050 - 0.0010 %
Copper, Cu 0.00010 - 0.00020 %
0.00010 - 0.00020 %
Indium, In 23.17 %
23.17 %
Iron, Fe 0.00010 - 0.00020 %
0.00010 - 0.00020 %
Lead, Pb 0.0010 - 0.0030 %
0.0010 - 0.0030 %
Magnesium, Mg 0.00010 - 0.0010 %
0.00010 - 0.0010 %
Nickel, Ni 0.0010 - 0.0020 %
0.0010 - 0.0020 %
Silicon, Si 0.00010 - 0.0010 %
0.00010 - 0.0010 %
Thallium, Tl 0.0010 - 0.0020 %
0.0010 - 0.0020 %
Tin, Sn 0.0010 - 0.0020 %
0.0010 - 0.0020 %