Material Notes:
Wave Solder Flux #66 is a completely organic, liquid flux containing non-evaporating vehicles and is suitable for tin and all conventional solder alloys. It incorporates a unique fluxing ingredient and offers an exceptionally high degree of activity in the soldering and tinning temperatures.Uses:Hot-dip tinning of brass and copper strip, ribbon or tapeSuitable for soldering to silver, lead, gold, tin-nickel (plate), tin (plate), cadmium, bronze and nickel.Physical Properties Flash point: noneInformation provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 1.06 - 1.10 g/cc

@Temperature 15.5 °C
1.06 - 1.10 g/cc

@Temperature 59.9 °F
Descriptive Properties Value Comments
Flash Point None
Users viewing this material also viewed the following: