Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. 3590-T Wave Solder Flux, No-Residue

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 3590-T Wave Solder Flux, No-Residue.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3590-T is a low-solids, non-halide rosin/resin free flux designed to eliminate post-cleaning operations. The effective flux activators provide superior solderability of surface mount, mixed technology and through-hole electronic assemblies.3590-T has a wide process window with excellent wetting capabilities, leaving no residue and high surface insulation resistance.FeaturesEliminates the need for cleaningExcellent wetting and solderabilityCompatible with conformal coatings without cleaningMeets Bellcore Specification TR-NWT-000078Meets IPC J-STD-004 Flux type ORL0Will not interfere with Pin TestingPhysical Properties Color: ClearFlux Type Classification: ORL0Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.801 g/cc

@Temperature 25.0 °C
0.801 g/cc

@Temperature 77.0 °F
0.808 g/cc

@Temperature 15.5 °C
0.808 g/cc

@Temperature 59.9 °F
Solids Content 1.85 %
1.85 %
Thermal Properties Metric English Comments
Flash Point 28.9 °C
84.0 °F
TCC
Electrical Properties Metric English Comments
Insulation Resistance 7.06e+13 ohm
7.06e+13 ohm
Control - initial; Standard Bellcore
8.11e+13 ohm
8.11e+13 ohm
Control - final; Standard Bellcore
9.96e+9 ohm

@Time 346000 sec
9.96e+9 ohm

@Time 96.0 hour
Control; IPC B25A
1.81e+10 ohm

@Time 86400 sec
1.81e+10 ohm

@Time 24.0 hour
Control; IPC B25A
Chemical Properties Metric English Comments
Acid Value 16
16
Copyright © lookpolymers.com All Rights Reserved