Indium Corp. 2632 Soldering Flux

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 2632 Soldering Flux.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
2632 is an alcohol-based flux developed for soldering can seams. 2632 provides fast wetting for dependable soldering and excellent seam-fill on tin-plated cans.FeaturesExcellent surface wetting on tin.Dries quicklyleaves minimal residuePhysical PropertiesColor: PaleInformation provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.864 g/cc

@Temperature 25.0 °C
0.864 g/cc

@Temperature 77.0 °F
0.871 g/cc

@Temperature 15.5 °C
0.871 g/cc

@Temperature 59.9 °F
Solids Content 20 %
20 %
Thermal Properties Metric English Comments
Flash Point 12.0 °C
53.6 °F
Chemical Properties Metric English Comments
Acid Value 66
66