Indium Corp. 1095-NF Wave Solder Flux, Water-Soluble

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 1095-NF Wave Solder Flux, Water-Soluble.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wave Solder Flux 1095-NF water-soluble flux is a neutral pH formulation with a high level of activity for wave soldering surface-mount, mixed-technology and through-hole electronic assemblies.1095-NF is biodegradable and cleans readily in water to low ionic levels, while leaving a surface which has a high surface insulation resistance.FeaturesHigh activity levelLow SolidsCleans to low ionic levelsCleaning can be delayed up to 48 hoursPhysical Properties Color: Clear to light yellowFlux Type Classification: ORH1Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.838 g/cc

@Temperature 25.0 °C
0.838 g/cc

@Temperature 77.0 °F
0.844 g/cc

@Temperature 15.5 °C
0.844 g/cc

@Temperature 59.9 °F
Solids Content 19.5 %
19.5 %
Thermal Properties Metric English Comments
Flash Point 12.2 °C
54.0 °F