Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Indium Corp. 1081-T Wave Solder Flux

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 1081-T Wave Solder Flux.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wave Solder Flux 1081-T is a water wash organic solder flux suitable for all conventional tin-lead alloys. 1081-T exhibits excellent solderability with low ionic residues after aqueous cleaning.FeaturesExcellent solderabilityWide process windowCleans to low ionic levelsPhysical Properties Color: Light AmberFlux Type Classification: ORH0Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.908 g/cc

@Temperature 25.0 °C
0.908 g/cc

@Temperature 77.0 °F
0.913 g/cc

@Temperature 15.5 °C
0.913 g/cc

@Temperature 59.9 °F
Solids Content 12.57 %
12.57 %
Thermal Properties Metric English Comments
Flash Point 20.0 °C
68.0 °F
TCC
Copyright © lookpolymers.com All Rights Reserved