Indium Corp. 1025 Water-Soluble Wave Solder Flux

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 1025 Water-Soluble Wave Solder Flux.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Wave Solder Flux 1025 is a highly active, versatile, water-soluble wave flux formulated to maximize yields and reduce defects on surface-mount and mixed-technology assemblies. It has a broad processing range and provides excellent wetting.14 Rosin Flux can be applied by foam, dip, wave or spray fluxing equipment. If thinning is required, use 16-1020 flux thinner to maintain specific gravity during use.FeaturesHigh activityLow SolidsLeaves shiny solder jointsCleans to low ionic levelsPhysical Properties Color: Light Straw ColorFlux Type Classification: ORH1Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc

@Temperature 25.0 °C
0.952 g/cc

@Temperature 77.0 °F
0.956 g/cc

@Temperature 15.5 °C
0.956 g/cc

@Temperature 59.9 °F
Solids Content 19.76 %
19.76 %
Thermal Properties Metric English Comments
Flash Point 12.2 °C
54.0 °F