Imerys ImerPlastâ„¢ 20 Recycled Polyolefin for Pipe Extrusion

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyolefin
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name ImerPlast™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys ImerPlastâ„¢ 20 Recycled Polyolefin for Pipe Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Stiffness Polyolefin/Mineral CompoundInformation provided by Imerys.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength 23.0 MPa
3340 psi
Flexural Modulus 1.00 GPa
145 ksi
Processing Properties Metric English Comments
Moisture Content 0.05 %
0.05 %
as packed
Descriptive Properties Value Comments
Color Dark Gray
Melt Filtration 240 µm