Imerys ImerPlastâ„¢ 10WPCT Recycled Polyolefin Resin

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyolefin
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name ImerPlast™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys ImerPlastâ„¢ 10WPCT Recycled Polyolefin Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A black, UV stabilized, recycled resin with no significant odor, for compounding with wood flour for extruded decking applications. With added reinforcing filler and wood flour dispersant, ImerPlastTM 10WPCThas been shown to significantly improve extruder output. Melt filtered to 250 µm to ensure no particulates.Information provided by Imerys.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
Melt Flow 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
2.0 g/10 min

@Load 5.00 kg,
Temperature 230 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Mechanical Properties Metric English Comments
Tensile Strength 22.0 MPa
3190 psi
Tensile Modulus 1.60 GPa
232 ksi
Processing Properties Metric English Comments
Moisture Content 0.05 %
0.05 %
as packed
Descriptive Properties Value Comments
Color Dark Gray
Melt Filtration 250 µm