Material Notes:
Barden R is a Hydrated Aluminum Silicate available as an Air Float Beneficiated Fine Powder. This kaolin product is used as a high surface area “hard” filler for agricultural purposes.Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Brightness 70 - 80 %
70 - 80 %
% Reflectance
Oil Absorption 33 - 38 %
33 - 38 %
g/100g clay
Particle Mesh Size 325 Mesh
325 Mesh
1% retained
pH 4.0 - 5.5
4.0 - 5.5
Specific Surface Area 22 - 26 m²/g
22 - 26 m²/g
Component Elements Properties Metric English Comments
Al2O3 38.1 %
38.1 %
Fe2O3 1.6 %
1.6 %
Quartz 1.5 - 3.8 %
1.5 - 3.8 %
SiO2 45.1 %
45.1 %
Descriptive Properties Value Comments
Color white
Heating Loss (% max as produced) 1
at 105°C