Imerys #6 Tileâ„¢ Kaolin

Category Ceramic , Clay , Kaolin Clay , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys #6 Tileâ„¢ Kaolin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
#6 Tile is a high plasticity kaolin. It is well known for its contribution to high unfired strength plasticity and white fired properties. Information provided by Imerys.
Physical Properties Metric English Comments
Particle Size 2.0 µm
2.0 µm
60% finer than
Particle Mesh Size 325 Mesh
325 Mesh
0.5% retained
pH 6.5
6.5
Specific Surface Area 20 m²/g
20 m²/g
Component Elements Properties Metric English Comments
Al2O3 38.1 %
38.1 %
CaO 0.30 %
0.30 %
Fe2O3 0.50 %
0.50 %
K2O 1.4 %
1.4 %
Loss on Ignition(%) 13.5 %
13.5 %
MgO 0.40 %
0.40 %
Na2O 0.10 %
0.10 %
SiO2 45.5 %
45.5 %
Descriptive Properties Value Comments
M.B.I. (meq/100g) 9.8