Material Notes:
Information provided by ITW Devcon
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0400 lb/in³
Viscosity 12000 cP
12000 cP
Mixed Viscosity
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
Cured; ASTM D2240
Tensile Strength at Break 22.8 MPa
3300 psi
ASTM D412
Elongation at Break <= 350 %
<= 350 %
ASTM D412
Tear Strength 90.3 kN/m
515 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 88
88
H-18 wheel (1000 gram load)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
wet
177 °C
350 °F
dry
Shrinkage 0.14 %
0.14 %
Cured; ASTM D2566
Electrical Properties Metric English Comments
Dielectric Strength 13.8 kV/mm
350 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 60.0 min
1.00 hour
Functional cure
Pot Life 3.00 min

@Temperature 23.9 °C
3.00 min

@Temperature 75.0 °F
Descriptive Properties Value Comments
Coverage per pound, in² @ 1/4" thickness 100
Mix ratio by weight (Resin:Hardener) 80:20