ITW Devcon Flexane® Rubber Repair / Castable Urethane Brushable, Black

Category Polymer , Adhesive , Thermoset , Polyurethane, TS
Manufacturer ITW Devcon
Trade Name Flexane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Devcon Flexane® Rubber Repair / Castable Urethane Brushable, Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by ITW Devcon
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0385 lb/in³
Viscosity 40000 cP
40000 cP
Mixed Viscosity
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
Cured; ASTM D2240
Tensile Strength at Break 24.1 MPa
3500 psi
ASTM D412
Elongation at Break <= 600 %
<= 600 %
ASTM D412
Tear Strength 70.1 kN/m
400 pli
ASTM D624
Taber Abrasion, mg/1000 Cycles 90
90
H-18 wheel (1000 gram load)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 48.9 °C
120 °F
wet
82.2 °C
180 °F
dry
Shrinkage 23 %
23 %
Cured (shrinkage due to solvent loss); ASTM D2566
Electrical Properties Metric English Comments
Dielectric Strength 13.4 kV/mm
340 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 1440 min
24.0 hour
Functional cure
Pot Life 45.0 min

@Temperature 23.9 °C
45.0 min

@Temperature 75.0 °F
Descriptive Properties Value Comments
Coverage per pound, in² @ 1/4" thickness 104
Mix ratio by weight (Resin:Hardener) 80:20