IRPC Polimaxx Porene SP100 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer IRPC Polimaxx
Trade Name Porene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Porene SP100 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:injection moldinghelmetsautomotive
Physical Properties Metric English Comments
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110

@Thickness 6.35 mm,
Temperature 23.0 °C
110

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D785
Tensile Strength, Ultimate 44.1 MPa

@Temperature 23.0 °C
6400 psi

@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 63.7 MPa

@Temperature 23.0 °C
9250 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 2.16 GPa

@Temperature 23.0 °C
313 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 3.33 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
6.25 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C

@Thickness 6.35 mm
194 °F

@Thickness 0.250 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °C

@Thickness 6.35 mm
183 °F

@Thickness 0.250 in
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in