IRPC Polimaxx Porene AN510 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer IRPC Polimaxx
Trade Name Porene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Porene AN510 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:injection moldingelectrical appliances such as microwaves, computers, tv, switch boxes, switch panels, etc.automotive componenets
Physical Properties Metric English Comments
Melt Flow 5.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
5.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 108

@Thickness 6.35 mm,
Temperature 23.0 °C
108

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D785
Tensile Strength, Ultimate 48.1 MPa

@Temperature 23.0 °C
6970 psi

@Temperature 73.4 °F
ASTM D638
Flexural Yield Strength 64.7 MPa

@Temperature 23.0 °C
9390 psi

@Temperature 73.4 °F
ASTM D790
Flexural Modulus 2.21 GPa

@Temperature 23.0 °C
320 ksi

@Temperature 73.4 °F
ASTM D790
Izod Impact, Notched 0.981 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C

@Thickness 6.35 mm
183 °F

@Thickness 0.250 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C

@Thickness 6.35 mm
174 °F

@Thickness 0.250 in
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
V-0

@Thickness 3.10 mm
V-0

@Thickness 0.122 in