Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IRPC Polimaxx Polene V1160 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene V1160 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: GOOD FLOWABILITYAPPLICATIONS: INJECTION MOLDING FOR LIGHT WEIGHT HOUSEHOLDS, TOYS, FOOD CONTAINERS, COSMETICS CLOSURES, DISPOSABLE ARTICLES, LARGE MOLDING AND COMPLICATED PARTS
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 3.0 hour
>= 3.0 hour
Condition B, F50; ASTM D1693
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 190 °C
15 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
43 g/10 min

@Load 5.00 kg,
Temperature 190 °C
43 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65.5
65.5
DIN 53505
Tensile Strength at Break 13.5 MPa
1960 psi
ASTM D638
Tensile Strength, Yield 29.0 MPa
4210 psi
ASTM D638
Elongation at Break 130 %
130 %
ASTM D638
Charpy Impact, Notched 0.250 J/cm²
1.19 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 170 - 250 °C
338 - 482 °F
Copyright © lookpolymers.com All Rights Reserved