Material Notes:
CHARACTERISTICS: HIGH MOLECULAR WEIGH FOR BLOW MOLDING GRADE, RIGID, STACKABLE AND HIGHLY SHOCK RESISTANT CONTAINERS, EXCELLENT IMPACT STRENGTH APPLICATIONS: BLOW MOLDING FOR L-RING DRUMS (200 LITRES), OPEN TOP DRUMS (120 LITRES) PACKAGINGS ALL TYPE OF HAZADOUS MATERIALS
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D792
Environmental Stress Crack Resistance 165 hour
165 hour
Condition B, F50; ASTM D1693
Melt Flow 0.080 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.080 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
1.8 g/10 min

@Load 21.6 kg,
Temperature 190 °C
1.8 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
DIN 53505
Tensile Strength at Break 50.0 MPa
7250 psi
ASTM D638
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 1750 %
1750 %
ASTM D638
Charpy Impact, Notched NB
NB
DIN 53453
Thermal Properties Metric English Comments
Vicat Softening Point 130 °C
266 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 170 - 250 °C
338 - 482 °F
Users viewing this material also viewed the following: