Material Notes:
CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 20% GLASS FIBRE REINFORCED, HIGH IMPACT STRENGTH, HIGH MECHANICAL STRENGTH, HIGH STIFFNESS, LOW SHRINKAGEAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 97
97
ASTM D785
Tensile Strength, Yield 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Yield Strength 58.8 MPa
8530 psi
ASTM D790
Flexural Modulus 4.70 GPa
682 ksi
ASTM D790
Izod Impact, Notched 0.647 J/cm

@Temperature 23.0 °C
1.21 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
ASTM D648