IRPC Polimaxx Pentfoam 455E Expandable Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer IRPC Polimaxx
Trade Name Pentfoam
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Pentfoam 455E Expandable Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GENERAL: PENTFOAM "455E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST CYCLES IN VACUUM MOLDING MACHINES AND CONVENTIONAL MOLDING MACHINES.APPLICATIONS: PENTFOAM "455E" IS PARTICULARLY WELL SUITED FOR THE MANUFACTURE OF EPS PACKAGING PRODUCTS, WITH PART WALL THICKNESS LESS THAN 10 MM. AND WHERE SE PROPERTIES ADVANTAGEOUS. SE GRADES CAN GENERALLY NOT BE USED IN FOOD PACKAGING.
Physical Properties Metric English Comments
Density 0.0160 - 0.0170 g/cc
0.000578 - 0.000614 lb/in³
0.0240 - 0.0400 g/cc
0.000867 - 0.00145 lb/in³
molding density range
Bead Size 0.400 - 0.710 mm
0.0157 - 0.0280 in
Maximum Moisture Content 0.20
0.20
Mechanical Properties Metric English Comments
K Factor (Wear Factor) 54 - 58
54 - 58
Chemical Properties Metric English Comments
Blowing Agent Content >= 5.3 %
>= 5.3 %