Material Notes:
CORROSION - (Patent pending). Versatile family of compounds designed for pressurized and thermo-mechanically stressed applications. Excellent corrosion resistance and high strength.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Water Absorption 0.080 %
0.080 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 40 - 50
40 - 50
ASTM D2583
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 13.0 GPa
1890 ksi
ASTM D790
Compressive Strength 186 MPa
27000 psi
ASTM D695
Izod Impact, Notched 7.60 J/cm
14.2 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 16.9 kV/mm
429 kV/in
ASTM D149