Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IDI Composites 46-16 Thermoset Polyester, Molding

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer IDI Composites
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IDI Composites 46-16 Thermoset Polyester, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Premium high strength electrical grade with excellent resistance to smoke generation, weathering, and corrosive environments.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Water Absorption 0.15 %
0.15 %
in 24 hours; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Barcol 45 - 55
45 - 55
ASTM D2583
Tensile Strength, Ultimate 55.0 MPa
7980 psi
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Compressive Strength 179 MPa
26000 psi
ASTM D695
Izod Impact, Notched 8.90 J/cm
16.7 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Electrical Properties Metric English Comments
Dielectric Strength 11.4 kV/mm
290 kV/in
ASTM D149
Arc Resistance 187 sec
187 sec
ASTM D495
Users viewing this material also viewed the following: