IDI Composites 44-10 HGM Thermoset Polyester, Molding

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer IDI Composites
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IDI Composites 44-10 HGM Thermoset Polyester, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Same as 44-10 HG with Mil Spec MAI-60.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.83 g/cc
0.0661 lb/in³
Water Absorption 0.24 %
0.24 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Compressive Strength 155 MPa
22500 psi
ASTM D695
Izod Impact, Notched 6.30 J/cm
11.8 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495