I. Stern PS2110 General Purpose Crystal Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Heat Resistant Grade
Manufacturer I. Stern & Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern PS2110 General Purpose Crystal Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Moderately High Heat ResistanceUL Classification 94 HBExcellent Water ClarityApplicationsDisplaysHouse waresInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Melt Flow 3.4 g/10 min
3.4 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.377 GPa
344.8 ksi
ASTM D790
Izod Impact, Notched 0.214 J/cm
0.400 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C
195 °F
ASTM D648
Vicat Softening Point 96.1 °C
205 °F
ASTM D1525
Flammability, UL94 HB
HB