Material Notes:
Features:Excellent ClarityExcellent Process PropertiesHigh Heat MoldingApplicationsMedical PartsDomestic AppliancesAgency RatingsFDA Title 21 CFR 177.1640UL File E220962Information provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Melt Flow 3.8 g/10 min
3.8 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 75.2 MPa
10900 psi
ASTM D790
Flexural Modulus 3.25 GPa
471 ksi
ASTM D790
Izod Impact, Notched 0.406 J/cm
0.760 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 91.1 °C
196 °F
ASTM D648
Vicat Softening Point 91.1 °C
196 °F
ASTM D1525
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in