I. Stern HIPS SH03 High Impact Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer I. Stern & Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern HIPS SH03 High Impact Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:High flowExcellent toughnessExcellent processabilityApplicationsInjection moldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.6 MPa
3130 psi
ASTM D638
Elongation at Yield 50 %
50 %
ASTM D638
Flexural Strength 36.3 MPa
5260 psi
ASTM D790
Flexural Modulus 1.77 GPa
256 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 76.1 °C
169 °F
ASTM D648
Vicat Softening Point 97.2 °C
207 °F
ASTM D1525